PHYSICAL ARC STUD WELDING TESTING

2014.09.12

PHYSICAL ARC STUD WELDING TESTING

BEND TEST: By striking the stud with a hammer, or by sliding a length of pipe or tube over the stud, the stud can be bent a minimum of 30 degree away from its axis, or until failure occurs. Satisfactorily welded studs should exhibit a complete 90 degree bend without failure.

TORQUE TEST : The stud may be torqued with conventional torque testing equipment by applying torque until a predetermined torque or proof load is reached or until failure occurs.

TENSILE TEST : The stud may be tested with conventional tensile testing equipment until a
predetermined load is reached or failure occurs.

OTHER : The stud and weld can be submitted to other conventional forms of destructive or non
-destructive testing as specifications may required.

We can make ceramic ferrule for stud welding according to your requirement.Also our ceramic ferrule has passed above test.(normally with shear connector)

ceramic ferrule for stud welding